Detailed analysis: how to produce digital crystal video Crafts

First of all, in need of handling a good photo PHOTOSHOP lined version, size A4. Print Resolution 300, with Epson R210 printer as an example; select items in the high quality option to choose which to print "photo quality", paper type selection <color durable photo paper> print output according to your needs for used ink some adjustments, the general is to deepen the color, the cyan, magenta, yellow, deeper points are appropriate, this has done to the crystal clear image quality will be better. This need to the actual circumstances of your ink set.

Transfer membrane is divided into pros and cons, printable surface and non-print side of the difference is that finger in the transfer of non-print area on the diaphragm light pull, feel will be very smooth, no feeling of hanging hand , in the printable surface with two fingers pinch as long as there will be obvious fingerprints on it, non-print area is not the case. To reduce printing costs, the printer can be used CISS. After the transfer printing patch, need to be dried hot hair dryer, make the printed transfer membrane surface be dry, because the transfer film has some of the sticky ink absorption, such as not fully dried, the production occurs during the transfer diaphragm can not move can not be required positioning. Dry knife can cut a piece of paper cut according to image size specifications to open, if you do not have cutting knife, utility knife is the same.

Out need to make crystal blanks, crystal blank sticky above, some debris and dust need to wipe clean, wipe the time to carefully. Transfer to be made good after the patch because the left exposed to print, sometimes the surface will be stained with dust, need to use a fingernail to gently above the glue get clean and dust debris carefully. Is fingernails, fingers can not touch, otherwise, would leave fingerprints. After a good glue coating, the transfer membrane face down into the crystal blank, the release time to smooth. You can see the glue through the membrane transfer under the film spread out, with a small scraper (after treatment with a small blade tape) in the middle of the glue from the glue separately, gently push forward, eyes looking at glue, glue did not come from a place where more than glue to glue the parts did not push. Good first half pushed, half post need to scrape, to glue evenly covered the entire crystal surface. Glue are in place to continue with a small spatula to transfer the excess glue patch release next. Carefully watching the screen, grasp the folded down glue action. Excess glue after full introduction of the crystal blank can promote special UV light box, the push time to careful not to touch transfer membrane, because the glue has not cured, touch that would be misplaced, and that the bubble will soon appear on the inside, and led to naught.

5-6 minutes, you can remove the semi-curing a good crystal, into the board, with a knife along the circle around the program, the excess part of crystal blank film based off, and then along a corner peeled off the substrate, we can see that image has been on the transfer to the crystal.

Now into the next process, the crystals back Nianshang Qu. Crystal's back was a thin, high density material is advanced optical glass, get the time to be careful. Debris on the sheet, dust wipe. Sticky sheet of adhesive and glue stick pictures is not the same, in order to distinguish, sticky glue sheet packing is a cylinder. Note that coating of water action, you need to pay attention to how to distribute the glue on the crystal. Note that the hand moves up sheet, let down the left or right side, then slowly down the sheet, lay down hard in the middle finger after the extrusion sheet, so that the glue to spread around, if not to the local glue on the front move sheet, so that no glue where the glue to flow. Well after the need for glue distribution location, the blank sheet with the following crystal alignment. After alignment as the glue that time has not yet solidified in liquid form, flakes, there may be sliding, which requires hand on, so let the light in the ultraviolet at about 20 seconds before they can release the handle, then push to the UV light box internal.

About 10 minutes later, we can remove the semi-solidified crystal. At this time we can see, behind the thin crystal blanks slightly larger than the point, can often thin case is slightly larger than the crystal blank, so this can not be regarded as a finished product, the following need to be polished crystal handle, so blank become a real crystal crafts.

I am China Manufacturers writer, reports some information about air ambulance helicopter , electric tricycle.

Processing your request, Please wait....

Leave a Reply